SELECTION OF PRODUCTS ACCORDING TO THE PARAMETERS

Physical condition when delivered
Thermal and additional treatment
Presence of plastifying agent
Method of laying, compacting, application
Reference document for product properties
Filter result:
products found: 9
SELECT id, txt, site.txt_lang(txt, 3) as mark FROM products_marks WHERE type = 2 AND id IN (SELECT pm.id FROM products_marks pm, mark_properties mp WHERE pm.id = mp.mark AND property = 27 AND value IN (197,208)) AND hidden IS false ORDER BY mark LIMIT 5 OFFSET 0

MC

Type: zirconium
Group: zircon
Refractoriness value: fire resistance (1580 to 1770°С)
Grain size: micro-grained
Physical condition when delivered: semidry
Thermal and additional treatment: thermo-hardening
Presence of plastifying agent: plasticized
Method of laying, compacting, application: casting
Group, depending on intended purpose: fire resistant mortars
Intended purpose: for binding of zircon products in refractory laying

MCM-1

Type: zirconium
Group: alumino-oxide zirconium-silicious
Grain size: micro-grained
Physical condition when delivered: semidry
Thermal and additional treatment: thermo-hardening
Presence of plastifying agent: plasticized
Method of laying, compacting, application: casting
Group, depending on intended purpose: fire resistant mortars
Intended purpose: for binding of zircon-mullite products in refractory laying

MCM-2

Type: zirconium
Group: alumino-oxide zirconium-silicious
Refractoriness value: fire resistance (1580 to 1770°С)
Grain size: micro-grained
Physical condition when delivered: semidry
Thermal and additional treatment: thermo-hardening
Method of laying, compacting, application: casting
Group, depending on intended purpose: fire resistant mortars
Intended purpose: for binding of zircon-mullite products in refractory laying

MDC

Type: zirconium
Group: oxide zirconium
Refractoriness value: fire resistance (1580 to 1770°С)
Grain size: micro-grained
Physical condition when delivered: semidry
Thermal and additional treatment: thermo-hardening
Presence of plastifying agent: plasticized
Method of laying, compacting, application: casting
Group, depending on intended purpose: fire resistant mortars
Intended purpose: for binding of zirconia products in refractory laying

MKC

Type: zirconium
Group: alumino-oxide zirconium-silicious
Refractoriness value: fire resistance (1580 to 1770°С)
Grain size: micro-grained
Physical condition when delivered: semidry
Thermal and additional treatment: thermo-hardening
Presence of plastifying agent: plasticized
Method of laying, compacting, application: casting
Group, depending on intended purpose: fire resistant mortars
Intended purpose: for binding of alumina-zircon products in refractory laying